Post by ayard »

Hi,

This question is mostly for my curiosity .... I notice that the Proteus boards prior to 0.6 (and maybe 0.5, I don't have a 0.5 here) were finished in what appears to be HASL. The 0.6 board appears to be a gold finish, is this an ENIG or an ENEPIG finish? Is the gold finish only for the Tag-Connect JTAG connector, or were there other reasons for this?

Al
mck1117
running engine in first post
running engine in first post
Posts: 1494
Joined: Mon Jan 30, 2017 2:05 am
Location: Seattle-ish

Re: PCB finish

Post by mck1117 »

ENIG is both easier to solder and more corrosion resistant.